Bulk Fill Composite Resins. A Novelty in Resin-Based Restorative Materials

Dr. Dimitrios Dionysopoulos

Department of Operative Dentistry, School of Dentistry, Aristotle University of Thessaloniki, Thessaloniki, Greece.

Citation : Dimitrios D. Bulk Fill Composite Resins. A Novelty in Resin-Based Restorative Materials. ARC Journal of Dental Science. 2016;1(2):1–3.DOI: dx.doi.org/10.20431/2456-0030.0102001

Copyright : © 2016 Dimitrios D. This is an open access article distributed under the Creative Commons Attribution License, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.

Abstract


Composites resins are the most popular restorative materials providing very good esthetics and long period of good clinical performance. Depth of cure of composite resins is crucial in determining the maximal increment thickness when restoring tooth cavities. In restorations with conventional composite resins the thickness of each increment has been defined as up to 2 mm. Bulk fill composite resins are assumed to be curable to a thickness of 4-5 mm, develop lower polymerization shrinkage stresses and present higher light transmission properties due to reduction of light scattering at the filler–matrix interface by either decreasing the filler amount or increasing the filler size. Further studies especially in vivo are necessary to verify the improved clinical performance of bulk fill composite resins.




Composites resins are the most popular restorative materials providing very good esthetics and long period of good clinical performance. Depth of cure of composite resins is crucial in determining the maximal increment thickness when restoring tooth cavities. In restorations with conventional composite resins the thickness of each increment has been defined as up to 2 mm [1]. This limitation is related to the degree of monomer conversion of composite materials, which determines their mechanical and physical properties such as strength, modulus, hardness and solubility [2], as well as their biocompatibility [3]. Although the critical threshold for the degree of conversion of dental composite materials has not yet been established, it has been accepted that the degree of monomer conversion below 55% is not appropriate for clinical performance [4].

There are many parameters that affect depth of cure of composite resins. These contain composition (monomers, inorganic fillers, photoinitiators, coupling agents) [5-7], shade and translucency [8] of the composite resin and characteristics of the light-curing unit (LCU) such as light intensity, thermal emission, wave length range, diameter of the tip and curing mode [9]. Other factors such as exposure time [10] and distance of the restorative from the tip of the LCU [11] may also affect depth of cure of composite materials.

As it mentioned before, composite resins should be applied to the cavity only in increments up to 2 mm thick to ensure appropriate light transmittance and adequate degree of polymerization1. Nevertheless, incremental technique for composite restorations is associated with various weaknesses including the risk of incorporating air bubbles or contaminations between composite layers, failures in bonding between the increments and an extended treatment time [12].

Aiming to overcome these disadvantages and simplify the time-consuming incremental technique of composite restorations, a new category of composite restorative materials has been introduced the so-called “bulk fill” composite resins. Bulk fill composite resins are assumed to be curable to a thickness of 4-5 mm [13], develop lower polymerization shrinkage stresses [14] and present higher light transmission properties due to reduction of light scattering at the filler–matrix interface by either decreasing the filler amount [5] or increasing the filler size [15]. To achieve this extended depth of cure bulk fill composite resins have acquired certain modifications in their composition in order to increase penetration of visible light through the materials such as increased filler size [15] and novel photoinitiators [16].

It has been reported that a reduction in intermolecular distance from 0.3-0.4 nm to 0.15 nm may occur during polymerization of composite resins [17] generating stresses due to the contraction of the material, which may lead to bonding failure and increase in microleakage of the restoration. Previous studies have reported that bulk fill composite resins may present better polymerization shrinkage stress kinetics [18] and decreased cuspal deflection [19] than conventional composite resins. However, the improved behavior of these newly introduced composite restoratives concerning marginal adaptation to cavity walls remains unconfirmed [19].

Bulk fill composite resins are further classified into high-viscosity and low-viscosity (flowable) materials. High-viscosity bulk fill composites include greater amounts of filler particles compared to low-viscosity bulk fill composites. As a result, the flowable composite resins exhibit better adaptation on the cavity walls but present greater polymerization shrinkage and lower mechanical properties. Due to their lower mechanical properties their restorations is recommended to be finished with a 2-mm capping layer of a high-viscosity bulk fill composite resin, especially when restoring areas which are submitted to occlusal stresses [20].

It has been demonstrated that preheated composite resins show reduced viscosity [21] and increased polymerization efficiency [22]. Heating composite resins prior to placement in the cavity and immediately light-curing increases monomer conversion rate and thus the duration of the irradiation period may be decreased [22]. With increased paste temperature, free radicals and developing polymer chains become more fluid as a result of reduced paste viscosity and they react to a greater extent, leading to a more complete polymerization reaction and enhanced cross-linking [23]. The increase in the degree of polymerization of composite resins may lead to better internal adaptation to cavity walls [24], improved mechanical properties and increased wear resistance [22]. In a recent study [25] it has been demonstrated that pre-heating significantly reduces shrinkage force formation of high-viscosity bulk-fill and conventional composite resins, while maintaining or increasing the degree of monomer conversion, dependent upon the specific composite material used.

In conclusion, bulk fill composite materials may be very useful for restorations of posterior teeth mainly due to their advantages in application technique and polymerization shrinkage. However, further studies especially in vivo are necessary to verify the improved clinical performance of bulk fill composite resins.


References


  1. Sakaguchi R.L., Douglas W.H., Peters M.C., Curing light performance and polymerization of composite restorative materials, J. Dent. 20, 183-188 (1992).
  2. Ferracane J.L., Mitchem J.C., Condon J.R., Todd, R, Wear and marginal breakdown of composites with various degrees of cure, J. Dent. Res. 76, 1508-1516 (1997).
  3. Sideridou I.D., Achilias, D.S., Elution study of unreacted Bis-GMA, TEGDMA, UDMA, and Bis-EMA from light-cured dental resins and resin composites using HPLC, J. Biomed. Mater. Res. B Appl. Biomater. 74, 617-626 (2005).
  4. Silikas N., Eliades G., Watts D, Light intensity effects on resin-composite degree of conversion and shrinkage strain, Dent. Mater. 16, 292-296 (2000).
  5. Amirouche-Korichi A., Mouzali M., Watts D.C., Effects of monomer ratios and highly radiopaque fillers on degree of conversion and shrinkage-strain of dental resin composites, Dent. Mater. 25, 1411-1418 (2009).
  6. Sideridou I.D., Karabela M.M., Effect of the structure of silane-coupling agent on dynamic mechanical properties of dental resin-nanocomposites, J. Appl. Polym. Sci. 110, 507-516 (2008).
  7. Lizymol P.P., Kalliyana Krishnan V. A, comparison of efficiency of two photoinitiators for polymerization of light-cure dental composite resins, J. Appl. Polym. Sci. 107, 3337-3342 (2007).
  8. Theodoridis M., Dionysopoulos D., Koliniotou-Koumpia E., Dionysopoulos P., Gerasimou P., Effect of preheating and shade on surface microhardness of silorane-based composites, J. Investig. Clin. Dent. doi: 10.1111/jicd.12204 (2016).
  9. Torno V., Soares P., Martin J.M., Mazur R.F., Souza E.M., Vieira S. Effects of irradiance, wavelength, and thermal emission of different light curing units on the Knoop and Vickers hardness of a composite resin, J. Biomed. Mater. Res. B Appl. Biomater. 85, 166-171 (2008).
  10. Dionysopoulos D., Papadopoulos K., Koliniotou-Koumpia E., Effect of temperature, curing time and filler composition on surface microhardness of composite resins, J. Conserv. Dent. 18, 114-118 (2015).
  11. Dionysopoulos D., Koliniotou-Koumpia E., Kotsanos N., Dionysopoulos P, Correlation between depth of cure and distance between curing light tip and resin surface, Balk. J. Stom. 15:70-75 (2011).
  12. Flury S., Peutzfeldt A., Lussi A., Influence of increment thickness on microhardness and dentin bond strength of bulk fill resin composites, Dent. Mater. 30, 1104-1112 (2014).
  13. Dionysopoulos D., Tolidis K., Gerasimou P., Polymerization efficiency of bulk-fill dental resin composites with different curing modes, J. Appl. Polym. Sci. doi: 10.1002/app.43392 (2016).
  14. Marovic D., Taubock T.T., Attin T., Panduric V., Tarle Z., Monomer conversion and shrinkage force kinetics of low-viscosity bulk-fill resin composites, Acta Odontologica Scandinavica 73:474-480 (2015).
  15. Ilie N., Stark K., Curing behavior of high-viscosity bulk-fill composites, J. Dent. 42, 977-985 (2014).
  16. Moszner N., Fischer U.K., Ganster B., Liska R., Rheinberger, V., Benzoyl germanium derivatives as novel visible light photoinitiators for dental materials, Dent. Mater. 24, 901-907 (2008).
  17. Jenson M.E., Chan D.C.N., Polymerization shrinkage and microleakage. In: Vanherle, G., Smith, D.C., editors. Posterior composite resin dental restorative materials. Utrecht, the Netherlands, Peter Szulc Publishing Co., pp. 243-262 (1985).
  18. El-Damanhoury H., Platt J., Polymerization shrinkage stress kinetics and related properties of bulk-fill resin composites, Oper. Dent. 39, 374-382 (2013).
  19. Moorthy A., Hogg C.H., Dowling A.H., Grufferty B.F., Benetti A.R., Fleming G.J., Cuspal deflection and microleakage in premolar teeth restored with bulk-fill flowable resin-based composite base materials, J. Dent. 40, 500-505 (2012).
  20. Bucuta S., Ilie N., Light transmittance and micro-mechanical properties of bulk fill vs. conventional resin based composites, Clin. Oral Investig. 18:1991-2000 (2014).
  21. Dionysopoulos D., Tolidis K., Gerasimou P., Koliniotou-Koumpia E., Effect of preheating on film thickness of contemporary composite restorative materials, J. Dent. Sci. 9:313-319 (2014).
  22. Dionysopoulos D., Tolidis K., Gerasimou P., The effect of composition, temperature and post-irradiation curing of bulk fill resin composites on polymerization efficiency, Mater. Res. doi: http://dx.doi.org/10.1590/1980-5373-MR-2015-0614 (2016).
  23. Daronch M., Rueggeberg F.A., De Goes M.F., Monomer conversion of pre-heated composite, J. Dent. Res. 84:663-667 (2005).
  24. Park S.H., Lee C.S., The difference in degree of conversion between light-cured and additional heat-cured composites, Oper. Dent. 21:213-217 (1996).
  25. Dionysopoulos D., Papadopoulos C., Koliniotou-Koumpia E., The evaluation of various restoration techniques on internal adaptation of composites in class V cavities, Int. J. Biomater. 2014:148057 (2014).
  26. Taubock T.T., Tarle Z., Marovic D., Attin T., Pre-heating of high-viscosity bulk-fill resin composites: Effects on shrinkage force and monomer conversion, J. Dent. 43:1358-1364 (2015).